Uneven mercerisation shows itself most obviously as

  • A.patchy dye uptake after dyeing
  • B.a marked change in the fabric weight
  • C.a serious loss of tensile strength
  • D.an unusually harsh handle only

Answer: A

The variation in accessibility translates directly into variation in shade, which the eye picks up readily. The fault often traces back to uneven impregnation or uneven tension across the width. The fault appears only after dyeing.