Discussion
If a precalciner completes 90 per cent of the calcination, what fraction remains for the rotary kiln to finish?
Answer: B
Correct answer: 10 per cent
\[ 100 - 90 = 10\ \mathrm{per\ cent}. \] Calcination is the most heat-hungry part of the process, so moving nine tenths of it out of the kiln and into the calciner is what allows a much shorter kiln to carry the same output - the kiln is left with the burning zone and little else.