Weld spalter is.......
Answer: C
Weld spatter is a welding defect.
Spatter is the droplets of molten metal thrown out of the arc that stick to the surface around the weld. It wastes filler metal and spoils the finish, and is usually caused by too high a current, too long an arc, wrong polarity or damp electrodes.
It is not a flux or an electrode coating, though a poor coating can increase spatter, and it is not a test; it is something inspection looks for.
No comment is present. Be the first to comment.
Loading…
Post your comment
Please log in or register to post a comment.
Examination Categories
- SSC Exams
- Banking Exams
- Teaching Exams
- Civil Services Exams
- Railways Exams
- Engineering Recruitment Exams
- Defence Exams
- State Government Exams
- Police Exams
- Insurance Exams
- Nursing Exams
- Other Government Exams
- NRA CET
- PG Entrance Exams
- Campus Placement
- MBA Entrance Exams
- CUET and UG Entrance
- Judiciary Exams
- Regulatory Body Exams
- Software Development